I am finally getting around to fitting solar panels after delays due to too much work and then a bad back for the last month. I have got all the bits so I am ready to go. BUT it is now getting cold and reading the Sikaflex 512 datasheet it says 'Application temperature 5°C to 35ºC'. Anyone got any experience of using Sikaflex at low temperatures? I suspect, looking at the graph, that it will just take longer to cure. Although even at 10°C 3mm thickness takes 4 days according to the graph.